‘Etching mill finish aluminum:
Fig. 4: The second last image from a sequence where a rolled aluminum surface
was etched in 85 % phosphoric acid at 55 °C for 15 s at the time. The irregular
white line at the image center shows the specimen drift during the experiment.
Etching mill finish aluminum
Kig. 5: The same topography file as in Fig. 4 but here centered laterally relative to
the first image in the sequence, and displayed as an “angle plot” with relief effect.
128